Standard curing agent for Polyester Resins and Gelcoats.
Im warmer conditions use minimum 1% by volume, i.e 10ml per Litre of Resin, never use less than 1%, in colder conditions use between 2-3%.
Always when catalyzing Gelcoats use 2% minimum.
Please handle very carefully, read safety data sheet and observe hazardous labelling.

Please note that due to its hazardous nature orders OF 5KG of MEKP catalyst and over can only be delivered on pallets. This will incur a higher delivery charge than shown by the website. Minimum pallet delivery charge is £70 + vat for Next Working Day and £56 + vat for 3 day delivery. We will attempt to contact you to arrange the excess payment and your order will be held until the payment is made.

Datasheets
Reviews (0)

Be the first to Write a Review for this item!

Video Guides
Q & A

Can I use less catalyst in warm or hot weather?

Never put any less than 1% catalyst in by volume, i.e 10 ml per Kg as this will affect the curing cycle and you run the risk of an under-cured laminate. You can get a slower reactivity catalyst though and this would extend the geltime whilst you are working.

Model
1629-1839
Brand
East Coast Fibreglass Supplies
East Coast Fibreglass Supplies